The nice part about Soda is it absorbs oil, and grease leaving a spot free
surface, I do it day in and day out we remove just about everything with it,
except Tape GOO, thats what laquer thinner is for!


----- Original Message -----
From: <[email protected]>
To: <[email protected]>
Sent: Tuesday, May 20, 2003 7:14 AM
Subject: Re: [TheForge] interesting project


> I am interested in this myself, since I have never had any luck
> sandblasting a '"soft" surface.   Even a clump of grease on an old
> autopart will defy the sandblaster.   Maybe my unit is too small, or I
> am too impatient.
>
> Charles
>
> terry l. ridder wrote:
>
> >hello;
> >
> >what type of equipment are we talking about here?
> >ordinary sandblasting equipment except using baking soda for media?
> >
> >On Mon, 19 May 2003, Paul Hewitt wrote:
> >
> >paul>
> >paul> Actually this is quite simple....
> >paul>
> >paul> Baking soda will solve all of your problems.  Find someone who does
baking
> >paul> soda blasting like me, and it can be done wet or dry, it will
remove the tar
> >paul> form all surfaces.   It will also remove any other contaminates
without
> >paul> etching or damaging them....paints etc.  I do it all the time, we
can ever
> >paul> remove graffiti, from soft sandstone brick surfaces with no damage.
It will
> >paul> not hurt the copper but may give it a nice shine which can be
etched with
> >paul> ammonia to restore the "patina" look.
> >paul>
> >paul> Baking soda can be swept up, broomed up then washed down with a
hose and its
> >paul> gone end of story, also its 100% EPA and DEQ legal.........
> >paul>
> >paul>
> >paul>
> >paul> You can email me directly @ [email protected]
> >paul>
> >paul> Paul Hewitt
> >paul>
> >paul> H&H Custom Solutions
> >paul>
> >paul>
> >paul>
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>