John Chobrda wrote: > > I want to make an open face die to forge a bunch of chisels. This die > will be used in the power hammer and/or hydraulic press. I am open to > suggestions as to the material to make this die from, all suggestions > are appreciated. How about 4140 or 4340. Tough as the devil and hard enough to work things hot.