> hmmm I always thought that any cast iron anvil was refered to as an ASO or
> anvil shaped object and that real anvils were wrought bodies or cast
steel,
> guess I was wrong huh
>
> PS
>  what makes those chinese ASO's so useless then?
>
>

They're just cast iron, no steel face.

They're not totally useless though; they're perfect for teaching a student
to hit the work NOT the anvil. Other than that they don't even make good
anchors. <grin>

Frosty
------------------------
If it ain't forged
it ain't real.
Wrought iron is.