[TheForge] Poor mans platen table

Shannell Sugrue [email protected]
Mon Mar 24 20:04:02 2003


I found a 3/4" 5' x 5' plate the other day at a used machinery place, with
looks like 1" square holes on a 5" grid. Would I loose anything using this
as a platen table, being only 3/4 thick I mean? Was $200, Id like a new work
table and this could be a good start.