From what Ive gathered, 10 to 1 is a good compromise, mines about 9:1, I
think 15:1 is optimal, above that is a waste, if I recall, anvil fire has a
little write up on this and what the commercial hammers use.
----- Original Message -----
From: "Jerry Frost" <[email protected]>
To: <[email protected]>
Sent: 23 March, 2003 12:53 PM
Subject: Re: [TheForge] Power hammer questions
> I'm contemplating a self contained hammer in the 100 lb. range.
>
> How heavy should the anvil be? Is there a ratio I can apply?
>