Much has been said about treadle hammers.  They can be as complex or as 
simple as you want.
Regarding treadle hammers, these are shots of the one I use daily.
It is based on the old abana plan (not the one referenced by D Mudge).
It has no adjustability. It has been used hard for over a decade.
It has 8 springs.  The energy required to use it is minimal because the
 eight springs are easier to extend than are fewer, larger springs.

http://www.artist-blacksmith.org/t-hammer1.jpg
http://www.artist-blacksmith.org/t-hammer2.jpg
http://www.artist-blacksmith.org/t-hammer3.jpg
http://www.artist-blacksmith.org/t-hammer4.jpg
http://www.artist-blacksmith.org/t-hammer5.jpg
http://www.artist-blacksmith.org/t-hammer6.jpg

This shot is of treadle hammer #2, same plan as above but stretched for 
an upcoming project.
Its head will be mounted on Monday.  Note the drift return slot on the 
side of the column.
Head weights on both are about 80lbs.
http://www.artist-blacksmith.org/t-hammer7.jpg

The work done on these very simple and cheap (I doubt there is $250 in 
either hammer) to build treadle
hammers  ranges from cold cut 18 & 16 gauge up thru hot cut 1/4" plate 
to hot slit
1" and 1 1/2" steel.  The chasing is cold into 3/16" and 1/8" steel.

http://www.artist-blacksmith.org/cold-cut.jpg
http://www.artist-blacksmith.org/cold-cut2.jpg
http://www.artist-blacksmith.org/cold-cut3.jpg
http://www.artist-blacksmith.org/hot-cut.jpg
http://www.artist-blacksmith.org/hot-cut/fullered.jpg
http://www.artist-blacksmith.org/hot-cut2.jpg
http://www.artist-blacksmith.org/hot-cut3.jpg
http://www.artist-blacksmith.org/hot-cut4.jpg
http://www.artist-blacksmith.org/hot-pierced.jpg

The work is done with tools like these.
http://www.artist-blacksmith.org/cutting_tools.jpg
S-1 and S-7 tools about 5" long.  The treadle hammer is not 
adjustable....never has that been an impediment.


Only two things matter in the world of treadle hammers;
does it work and are you happy with it.