Hi Chuck,
How are you balancing the cylinder travel?
Ed
----- Original Message -----
From: "chuck schaeffer" <[email protected]>
To: <[email protected]>
Sent: Wednesday, March 12, 2003 1:42 PM
Subject: Re: [TheForge] Hydraulic Forging Press
> Dave,
> I built and used a Batson design a few years back. In fact Ric has it in
> Sturgeion Bay with a few minor changes to it to meet his needs. It is a
> very good design and easy to built. The only thing, it had limitations un
> what you could used for.
>
> I now build H frame units as apposed to the C frame. The H frame allows
the
> pressure to go up by using two cylinders and still be under 3000 psi. The
> press I build now has foot control with automatic return when it reaches
> pressure with the option of being able to cycle it with a selected range.
> It develops a conservative 40 tons of force. The knifemakers at the ABANA
> conference used my H frame for their demos.
>
> If you would have more questions get back to me off line.
>
> Chuck
>
> Chuck Schaeffer
> Metals Magic Shop
> [email protected]
> Ph. 608.798.4296
> Fax 608.798.1940
>
>
> ----- Original Message -----
> From: "Dave Brown" <[email protected]>
> To: "TheForge" <[email protected]>
> Sent: Wednesday, March 12, 2003 12:03 PM
> Subject: [TheForge] Hydraulic Forging Press
>
>
> > I know there was a discussion about hydraulic presses a while back, but
I
> > wasn't interested then but I am now.
> >
> > Does anyone have any experience with the hydraulic forging press that
Jim
> > Batson
> > designed? (see:
> http://www.artmetal.com/project/TOC/BookRevu/HydroPrs.html )
> >
> > I know our good friend and occasional poster to theforge, Chuck
Schaeffer,
> > has considerable experience in this area. So, any comments and/or
> > suggestions will be appreciated from any and all.
> >
> > Also, does anyone remember when the discussion on hydraulics took place
on
> > this list so I can go back to the archives and look the postings up?
> >
> > Dave Brown
> > Heritage Smithing
> > Green Bay, WI
> > ABANA, UMBA, GoM, MODA, ARG
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>