At 09:23 AM 3/14/2003, you wrote:
>Ene bichizh ogsen baina shuu...
>
> > If you etch w/ muratic , you get a finish like that.
> >
> > Bet it's not "old". Huh?
> > dan tull
>
>That's what I was thinking- the bit about the "artistic twist" made me
>suspect somebody couldn't resist a certain amount of craftsman's pride ;-)
>
>But, it's a very interesting item. I saved the pictures, for a day when I
>decide to make something like that.
>
>Phlip
Yes, and the stock that it's made from looks like modern dimensional
material. Say, 1"x1/4" hot rolled? In addition take a look at the last
pic. If you look close it looks like a short modern arc-weld bead on the
most prominent hook near the bottom.
Dan Crowther
http://www.oakandacorn.com
http://home.nycap.rr.com/clancrowther