[TheForge] Viking Padlock

April and Bill Clemens [email protected]
Mon Mar 10 17:27:00 2003


Randy, 

The ones in the Mastermyr Find are:

10 lock body 4.5 x 3.0 x 2.2 cm  (1.77 x 1.18 x .87 in)
   shackle height 2.3 cm         (.9 in)

11 lock body 3.0 x 2.9 x 3.6 cm  (1.18 x 1.14 x 1.42 in)

12 lock body 2.8 x 2.2 x 2.6 cm  (1.1 x .87 x 1.02 in)

Bill Clemens

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of R.C.Mundt
Sent: Monday, March 10, 2003 2:17 PM
To: [email protected]
Subject: Re: [TheForge] Viking Padlock

About how big are these locks?
Randy Mundt
----- Original Message -----
From: "Robert Morris" <[email protected]>
To: <[email protected]>
Sent: Monday, March 10, 2003 9:48 AM
Subject: Re: [TheForge] Viking Padlock


> Dan,
>
> Are the books you mentioned obtainable? Can you send me the titles and
> where, if possible, I can get them.
>
> Bob M.
>
>
>
>
>
>
> >From: "irontree" <[email protected]>
> >Reply-To: [email protected]
> >To: <[email protected]>
> >Subject: Re: [TheForge] Viking Padlock
> >Date: Sun, 9 Mar 2003 16:41:28 -0600
> >
> >Bill
> >    I just got back from an SCA event where we discussed Viking
Locks!
> >...small world...I have several (3-4) books from various digs which
> >describe
> >the the locks and show pictures of how they worked.  I will try to
scan
in
> >the drawings and photos tonight.  If you want copies, I can post the
pages
> >online at my website or I can email them to you.
> >
> >Dan
> >
> >
> >-----Original Message-----
> >From: Dave Brown <[email protected]>
> >To: [email protected] <[email protected]>
> >Date: Saturday, March 08, 2003 8:13 PM
> >Subject: Re: [TheForge] Viking Padlock
> >
> >
> > >Bob,
> > >
> > >If you wouldn't mind, would/could you please post pictures of your
> >drawing
> > >of the works in theforge photoaccess site please.
> > >
> > >Dave Brown
> > >
> > >At 19:08 03/08/03 -0500, you wrote:
> > >>  Bill,
> > >>
> > >>  I'm not sure the people that wrote the description really
understood
> > >> every thing that the padlock showed. The rust build up on the
inside
of
> > >> the lock indicated there is three springs when they actually were
> >inside
> > >> wards with rust build up to appear like springs. I will talk to
you
at
> > >> the Furnacetown meeting and draw the operating works of the lock
so
you
> > >> can reproduce it.
> > >>
> > >>  Bob M.
> > >
> > >_______________________________________________
> > >http://mailman.qth.net/mailman/listinfo/theforge
> > >theforge mail list group photo site is
> > >http://www.photoaccess.com
> > >Login:  [email protected]
> > >password:  anvil
> > >___________
> > >
> > >
> >
> >
> >_______________________________________________
> >http://mailman.qth.net/mailman/listinfo/theforge
> >theforge mail list group photo site is
> >http://www.photoaccess.com
> >Login:  [email protected]
> >password:  anvil
> >___________
> >
> >
>
>
> _________________________________________________________________
> MSN 8 with e-mail virus protection service: 2 months FREE*
> http://join.msn.com/?page=features/virus
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>

_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  [email protected]
password:  anvil
___________