[TheForge] yurt wall connector, forge or cast?
Phlip
[email protected]
Sun Jun 29 19:00:01 2003
Terry, let me check with my SCA friends. I suspect that I could find you a
few websites that will answer all your questions- I get the distinct feeling
that you're over-engineering ;-)
BTW, the other name for yurt is "ger" pronounced "grrr", and spelled with
variations.
Phlip
"When in doubt, heat it up and hit it with a hammer."
Blacksmith's credo.
If it walks like a duck, and quacks like a duck, it is probably not a
cat.
Never a horse that cain't be rode,
And never a rider who cain't be throwed....
----- Original Message -----
From: "Terry L. Ridder" <[email protected]>
To: <[email protected]>
Sent: Saturday, June 28, 2003 1:33 AM
Subject: [TheForge] yurt wall connector, forge or cast?
> hello;
>
> i have been think over the wall connector for use in
> connecting the slats of a yurt wall together. i have
> mainly been focusing on how would i make several hundred
> of these in a reasonable amount of time. there seems to
> be two logical avenues to follow. forged using a series
> of dies or cast. this still leaves open what material
> would be used. stainless steel or brass or a monel alloy.