Did you try annealing them? Some nails are hardened. What type of nail did
you use?
-Carl Tappan
At 08:28 PM 6/10/03 -0600, you wrote:
>I've made a few rivets from nails when I didn't have the right length rivet.
>Found the nails I had were a bunch harder than store bought rivets.
>Randy Mundt
>----- Original Message -----
>From: "essayons" <[email protected]>
>To: <[email protected]>
>Sent: Tuesday, June 10, 2003 8:10 AM
>Subject: Re: [TheForge] rivets
>
>
>>
>>
>>
>> > I need a source for soft iron rivets. Got any ideas?
>>
>> Common nails are a good substitute.
>> Ed
>>
>> _______________________________________________
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: [email protected]
>> password: anvil
>> ___________
>>
>>
>>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________
>
>
>
http://www.bluetoadforge.com
"Gold for the mistress, silver for the maid.
Copper for the craftsman, cunning in his trade."
"Well," said the baron, sitting in his hall. "But iron, cold iron is the
master of them all."