When I used pea coke I had a round firepot cast from a Bruce LePage pattern.
A round firepot works the best for this fuel because you can mound the pea
coke in the forge better than a rectangular pot.
Bill
[email protected]
 http://home.centurytel.net/Fiorini_and_Skiles

----- Original Message -----
From: "Ralph & Charlaine" <[email protected]>
To: <[email protected]>
Sent: Saturday, June 07, 2003 6:46 AM
Subject: Re: [TheForge] Coke Fire Pot


> Roger Lorance
> 309-647-9242 Canton, IL
> [email protected]
>
>
>
> ----- Original Message -----
> From: "Roger R Degner" <[email protected]>
> To: <[email protected]>
> Sent: Saturday, June 07, 2003 10:24 AM
> Subject: Re: [TheForge] Coke Fire Pot
>
>
> > Roger Lowrence from Illinois also sell very heavy firepots.  I believe
> > Centaur resells his
> > Sorry I dont have an address for him.
> > www.umbaonline.org has a couple tapes if him demonstrating in there
> library.
> > He is a very talented smith
> > ----- Original Message -----
> > From: "Scott Lane" <[email protected]>
> > To: <[email protected]>
> > Sent: Thursday, June 05, 2003 11:32 PM
> > Subject: [TheForge] Coke Fire Pot
> >
> >
> > > Greetings,
> > > I am using pea size industrial coke in a forge with a normal coal fire
> > > pot.  While it is working for now I would prefer to get a coke fire
> > > pot.  The design of the clinker breaker in my current pot doesn't
allow
> me
> > > to rotate it with the coke, as the little bits are too hard to break
up
> > and
> > > just jam the whole thing...
> > > I recall that someone had coke fire pots for sale, but I can't track
> them
> > > down.
> > > Any suggestions?
> >
> >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  [email protected]
> > password:  anvil
> > ___________
> >
> >
> >
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>