Incralac comes in solvent and water based types now. The water based is =
actually a little harder than solvent and does not have the "nasty" =
solvents in it.
If you use a little you can get it from Talas (talasonline.com)=20
5 gal quantities can be purchased at a considerable savings over small =
quantities from Stan-Chem themselves (manufacturer).
If you order solvent, brace yourself for hazardous material charge. =
Another plus for water based (no HMC)
Buddy Holmes
Waterfall Forge
Waterfalling.com
Buddy Holmes
Waterfall Forge
--- StripMime Report -- processed MIME parts ---
multipart/alternative
text/plain (text body -- kept)
text/html
The reason this message is shown is because the post was in HTML
or had an attachment. Attachments are not allowed. To learn how
to post in Plain-Text go to: http://www.expita.com/nomime.html ---