You said hard coal as in anthracite? if your using that you need to add some kindling. Hard coal also takes more air to keep going which can be a problem. When your welding remember that your trying to suggest to the steel that they want to get together not force them together. Hit it too hard and all you do is splash out the metal that would form the weld.