[TheForge] Re: Advice? Air hammer die and anvil fit-up
Mike Spencer
[email protected]
Sun Jul 13 18:39:00 2003
larry> Would cutting the shoulder back on the die be an option?
ralph> Yes, it could be cut if it's not hardened. Grind or abrasive
ralph> cut if it is (would be possible), but the shim would be easier.
Yes indeed. And the die, despite some damage and pits, is more true
than the surfaces I've produces on the anvil. Be a shame to machine
the die cockeyed to match the anvil.
- Mike
--
Michael Spencer Nova Scotia, Canada
[email protected]
http://home.tallships.ca/mspencer/