[TheForge] Forging blackberries?
The Millers
[email protected]
Mon Jul 7 09:28:00 2003
It is relatively simple if you have casting/foundry capabilities.
Aluminum melts at about 1200 degrees and steel doesn't!!
I am taking an investment casting class and that is one of the
"techniques" being taught. You create your wax model of what you want
to cast in aluminum. It would include the steel strap. Then you
"invest" it in a plaster/sand mixture and then burnout the wax creating
the negative space for the aluminum. Melt the aluminum in a crucible,
pour it in the mold and TA DA!! (Hopefully)
We haven't poured anything yet. We are still making our wax models. We
are going to pour bronze and aluminum.
Ray Miller
Cincinnati
On Monday, July 7, 2003, at 01:25 AM, Shannell Sugrue wrote:
> Hey thats a trick worth knowing!
>
> ----- Original Message -----
> From: "RIES NIEMI" <[email protected]>
> To: <[email protected]>
> Sent: 07 July, 2003 1:48 PM
> Subject: Re: [TheForge] Forging blackberries?
>
>
>> on 7/6/03 8:37 PM, Shannell Sugrue at [email protected] wrote:
>>
>>> Yeah sorry they are blackberries, casting sounds better the more I
>>> think
> of
>>> it, Id probably cast them in Al but then have to think of a trick to
> attach
>>> them, mabey drill a hole and srew them onto the stems or
>>> similar(mabey
>>> epoxy) , there are no solders that can stick Al to steel are there??
>>>
>>
>> the big foundries that make aluminum ornamental panels for fences and
>> railings cast a steel weld tab right into the aluminum part. I am not
>> sure
>> how they do it, but I know that they do. A little piece of 1/4" x 1"
>> flat
>> bar, that sticks right out of the aluminum casting, and you just weld
>> it
>> right on your rinky dink square tubing framework, with your spattery
>> buzz
>> box that you dont know how to use.
>> If they can do it, then you probably could too. Or just get them to
>> do it-
>> Lawler foundry in Alabama is the biggest one, and I know they do
>> custom
> work
>> in both iron and aluminum.
>> www.lawlerfoundry.com/
>>
>> _______________________________________________
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: [email protected]
>> password: anvil
>> ___________
>>
>>
>>
>
> _______________________________________________