Ok this is what I did.=20
I put copper sulfate into warm water until it would hold no more.
I sand blasted the table and squirted it with phosphoric acid, let dry =
and then sprayed with the copper sulfate solution.
I put on 4 or 5 coats when each one dried.
It had bright copper on some places and dark brown or black in others. =
So I rubbed with scotch bright and most of the black rubbed off and some =
of the copper. I didn't really scrub it.
So am I doing it totally wrong or should do it again and just wipe it =
down and spray a clear coat over the mess?does it take some time to dry =
or cure? I was really going for the green copper effect.
Any assistance would be greatly appreciated.
Thanks
signed=20
Frustrated
--- StripMime Report -- processed MIME parts ---
multipart/alternative
text/plain (text body -- kept)
text/html
The reason this message is shown is because the post was in HTML
or had an attachment. Attachments are not allowed. To learn how
to post in Plain-Text go to: http://www.expita.com/nomime.html ---