There is a simple NO for that one, key shavings contain nickel plating, as
well as chrome, and other contaminates, also some keys are bronze, some are
aluminum, and some god only knows whets in them.
----- Original Message -----
From: <[email protected]>
To: <[email protected]>
Sent: Thursday, July 03, 2003 8:39 PM
Subject: Re: [TheForge] forge brazing
> how about shavings from a key cutting machine? Would that work for
brasing?
>
> Ralph Neumeister
> Maple Leaf Forge
> 17231 Messenger Rd.
> Burton, Ohio 44021
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed. To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>