The pieces are steel . I tried useing bronze sawdust (I cut a silicon bronze
ingot in half and collected the sawdust) where can you get powdered brass?
John
gblacksmith wrote:
> John: Are the pieces you are brazing of steel, bronze or brass? You did
> not specify. Forge brazing is often done with a material called spelter,
> which is essentially powdered brass. Recommended flux is pure anhydrous
> borax sprinkled on the pieces after the spelter is applied to the joint.
> avoid having the oxygen-rich gas flame hit the piece directly and place the
> piece so that he spelter will flow into the joint upon melting.
>
> Grant