I don't see any disrespect Steve. Heck, I haven't decided what to build I
just like knowing how these things work. I'm leaning towards a self
contained simply because I have almost everything I need to build one and
can buy what I don't have for less than the price of a decent compressor.

So, if anyone got the impression I think more of a self contained over a
Kinyon type, over a mechanical hammer I apologize for the poor
communications.

I was afraid something like machined flats was the case, something I don't
have the equipment to duplicate and I don't much care for external guides
either.

Thanks Steve.

Frosty
------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks

Meadow Lakes, AK.


----- Original Message -----
From: "Howell Steve" <[email protected]>
To: <[email protected]>
Sent: Wednesday, January 29, 2003 9:48 AM
Subject: RE: [TheForge] Hammer poll


> No disrepect, frosty-
> I have a 100lb. kinyon that I use a 5hp two stage 18cfm compressor on- it
hits upwards of 200 bpm at a short ~6" stroke. I put a picture of it on the
access site-
> The 3b is a 'light duty' 265 lb ram that runs at 180bpm, 10HP 1100 rpm
motor
> btw- the ram is a hollow bored forging that has machined flats on 4 sides
>
> Steve
> Seattle
>
>
> -----Original Message-----
> From: Jerry Frost [mailto:[email protected]]
> Sent: Tuesday, January 28, 2003 9:54 PM
> To: [email protected]; [email protected]
> Subject: [TheForge] Hammer poll
>
>
> As I was expecting, I didn't get enough responses to say anything
meaningful
> about horse power vs. ram weight/BPM.
>
> Thanks for participating.
>
> Frosty
> ------------------------
> If it ain't forged
> it ain't real.
> Wrought iron is.
> The FrostWorks
>
> Meadow Lakes, AK.
>
>
> ----- Original Message -----
> From: "Kevin" <[email protected]>
> To: "ArtMetal project" <[email protected]>
> Sent: Thursday, January 23, 2003 1:48 PM
> Subject: Fountains and other watery art stuff
>
>
> > While we're talking art fountains, you might be interested in:
> >
> > http://www.harriesheder.com/wwcamb.htm
> >
> > --
> >
> >
> > Kevin  (NW England, UK)
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
>   text/plain (text body -- kept)
>   text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment.  Attachments are not allowed.  To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html  ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>