george> 
george> Greetings,
george> I have used treadle hammers for well over a decade.  The ones I have 
george> built are the original 'abana plan' style machine, the plan for which 
george> was sold by abana in the late 80's.  It is one of the few which is not 
george> over-engineered.  The head has no accommodation for tooling. The head 
george> height is not adjustable and the head arcs....like a striker with a 
george> sledge hammer..... I have never looked at a treadle hammer as a leg 
george> powered "little giant'. 