The face should be hard. You also might need to grind a little off the face
to get rid of any metal that has the carbon burned out of it.
Darrell
----- Original Message -----
From: <[email protected]>
To: <[email protected]>
Sent: Saturday, January 18, 2003 1:21 PM
Subject: Re: [TheForge] Strikers
> So should the striker face be real hard or what?I made one from a high
carbon
> steel and hardened the face then tempered it somewhat so as not to be
brittle
> and could not get sparks.
>
> Bob
> HotAnvil Forge
> http://members.tripod.com/hotanvil_forge
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed. To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>