[TheForge] Sidearm burner parts
Shannell Sugrue
[email protected]
Wed Jan 15 05:51:00 2003
Yeah? sounds good, I can get 1 1/4 narrowing to 1", guess I could bush that
one then, I kind of thought a gradual taper would have been better than the
shoulder the bush must make?
----- Original Message -----
From: "Dan Scheid" <[email protected]>
To: <[email protected]>
Sent: 14 January, 2003 11:06 PM
Subject: Re: [TheForge] Sidearm burner parts
> I went with a 1 1/4 tee and then used bushing to get it down in size the
> current forge is welding at 6PSI
> Dan Scheid
> Flying horse forge
> http://home.earthlink.net/~chevalvolant/flyinghorseforge.html
> > Im having trouble finding a 1 1/4x 3/4 x 1 1/4 reducing T for my new
forge
> > burners here in Australia, are these comonly available elsewhere or is
> this
> > a very odd sized T?
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>