At 03:10 PM 1/12/03, you wrote:
I'd suggest a silicon or phosphor bronze..both are copper like in color and
significantly stronger...especially the phosphor bronze.
How bout a small decorative band to hold the S ends in place?//////Pete
>Go steel and paint it, there are some amazing copper paints available which
>even naturally patinate, indistinguishable from copper to me, I guess forged
>copper looks well "forged" though so that might be harder to replicate, tell
>him its cheaper and stronger and you should convince him.
>
>----- Original Message -----
>From: "H and P Foster" <[email protected]>
>To: "the forge" <[email protected]>
>Sent: 11 January, 2003 6:48 PM
>Subject: [TheForge] Here is a good question. Hard to believe also.
>
>
> >
> > A potential client is interested in me making some of my decorative chain
> > http://pages.infinit.net/rustydog/chain1.htm to hang his wifes new pot
>rack.
> > So far so good.
> >
> > He then says that the pot rack and cast iron pots will weigh 1000 pounds.
> > I write back asking if he put one too many zeros on his figure.
> > Nope......1000 pounds it is. He also wants the chain in copper.
> >
> > I suggested I make a few links out of 3/8" copper round stock and he can
> > have it tested for the load and that the responsibility will be his alone.
> > The rack will hang from 4 points.
> >
> > Do you think the copper of this dimension will be strong enough, or should
>I
> > suggest copper plated iron links instead?
> >
> > Thanks for any help or ideas.
> >
> >
> > Harry Foster
> > Rusty Dog Forge
> > http://pages.infinit.net/rustydog/home.htm
> >
> >
> >
> >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________