Beche: 15 hp    330lb ram       180bpm
Kenyon           110 lb ram      200+/- bpm
Kenyon            110lb.ram      200+/- bpm
Little giant  2hp  25lb ram       200++ bpm
Old Rivit hammer 15 lb ram    300bpm