>Some of you know that I already do a certain style of repoussÈ and chasing.
>I'm pleased with my skill level on that technique, but am trying to add more
>skills using thin-ish sheet metal. That's the best use of my skills and
>time- with 2 small children, limited shop time, and a need for paying
>commissions.
>
> I'm self-teaching/learning repoussÈd acanthus style leaves currently.
>Thanks to those of you who have sent me jpgs of Broussard tooling. I'm
>still waiting for some video rentals to come in through LAMA, but this is
>where I'm at with the technique right now.
>http://hosting.acegroup.cc/~koka/ornateleaves.jpg
>
>I'm getting a good feel for the technique, but do not feel like I can create
>every curve combination that I'd like. I'm also not getting the full
>rounded effect that I'd like in some areas.
>-Kirsten
>p.s. The drawing behind the leaves is not mine. I'm working for a designer
>on this project.
>[email protected]
>http://hosting.acegroup.cc/~koka/
>http://www.mnartists.org/?loc_name=viewartistfeature&artistid=2713
>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________