[TheForge] 1045 tools
George Dixon
[email protected]
Sun Feb 23 21:36:01 2003
On the Moon Lamp... Do you usually perform the repousse' prior to
or after cutting out the pattern (Im specifically asking about the star)...
The repousse' is done before the negative spaces are cut free. The
chasing of the repousse' along areas that will become drops is done with
chisels. This way the chasing of the volume and the cutting of the
negative spaces proceeds together.
If the pattern is cut out prior to repousse', then the relief cannot get
as bold.