[TheForge] joining al and steel
Raymond Miller
[email protected]
Fri Feb 21 19:35:59 2003
The only options I am aware of involve "soldering".
Ray Miller
Cincinnati
On Friday, February 21, 2003, at 05:16 PM, [email protected] wrote:
>
> Can aluminum and mild steel be fusion welded using a mig or oxy/act?
> Can they be welded using any process other than friction welding or
> explosive bonding?
> If so, how?
>
> TIA,