[TheForge] Brushed finish
Darrell
[email protected]
Thu Feb 13 19:51:00 2003
Bruce,
Thank you for the details. I knew what would happen, I just didn't know how
to explain it.
Darrell
http://www.machinemaster.com
----- Original Message -----
From: "Bruce Freeman" <[email protected]>
To: <[email protected]>
Sent: Thursday, February 13, 2003 11:07 AM
Subject: Re: [TheForge] Brushed finish
Because SS is not a uniform material. All SS that doesn't rust is
passivated. Literally, the iron is etched out of the surface, leaving
behind chromium and nickel. These form clear oxides - no rust. Cut through
this outer layer and expose the iron and bingo, rust.
Now wheter wire brushing WILL cut through this outer layer, I don't know.
(A mild steel wire brush deposits mild steel on SS, so that's a different
thing.) However, an abrasive pad certainly will cut through the outer
layer, because the abrasives they put on those things are much harder than
SS.
Bruce
NJ
>>> [email protected] 02/13/03 01:24PM >>>
Dan Scheid wrote:
>
> really, I thought that the property of stainless was in the material. Not
in
> the finish how fast will it rust ?
> Dan Scheid
>
> > Don't forget that roughing the surface of stainless can make it subject
to
> > rusting. If it will be exposed to the elements, it will either need to
be
> > coated or pasivated.
> > Darrell
How does a rough finish change the inherent property of SS? I know that
if you use a plain steel wire brush etc for the brushed look you can get
some particles of steel in the SS that will rust,, but if you use a SS
wire wheel you should not have this issue.
Ralph
"Good is the enemy of Excellent. Talent is not necessary for Excellence.
Persistence is necessary for Excellence. And Persistence is a Decision."
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: [email protected]
password: anvil
___________
_______________________________________________