really, I thought that the property of stainless was in the material. Not in
the finish how fast will it rust ?
Dan Scheid
> Don't forget that roughing the surface of stainless can make it subject to
> rusting. If it will be exposed to the elements, it will either need to be
> coated or pasivated.
> Darrell
>
> http://www.machinemaster.com
> ----- Original Message -----
> From: "Dan Scheid" <[email protected]>
> To: <[email protected]>
> Sent: Thursday, February 13, 2003 7:02 AM
> Subject: Re: [TheForge] Brushed finish
>
>
> > lol well I am planning on talking to a sandblaster friend of mine about
> that
> > Dan
> > ----- Original Message -----
> > From: "Dave Bendall" <[email protected]>
> > To: <[email protected]>
> > Sent: Thursday, February 13, 2003 5:56 AM
> > Subject: [TheForge] Brushed finish
> >
> >
> > > Hey, Dan, I had goofy idea for getting an even brushed finish on
> > > your sheet of stainless steel. Take it to a deserted dirt road, tie it
> > > to the bumper, and drag it a few miles.
> > >
> > > Dave Bendall in Phoenix
> > >
> > > _______________________________________________
> > > http://mailman.qth.net/mailman/listinfo/theforge
> > > theforge mail list group photo site is
> > > http://www.photoaccess.com
> > > Login: [email protected]
> > > password: anvil
> > > ___________
> > >
> > >
> > >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>