Mike,
Between the speed and the pine test, it sounds like you've pretty much =
confirmed my observations from 1998.
You could skip the see-saw mechanism, and simply balance the ram by a =
means similar to that used in the Weightless Eammer. I suspect the =
mechanism used in the Grasshopper Treadle Hammer might also work, but that =
was calculated for a slightly different mechanism than a swing-arm hammer, =
so I'm not sure.
Bruce
NJ
>>> [email protected] 02/10/03 01:51PM >>>
Well it belongs to a friend of mine I'm guessing a at a 10,15lb head and =
maybe twice that or a bit more on the back side.=20
he kinda just stuck it together, had to beef up the arm, 1-1/2" pipe, (it =
kept bending)
We stuck a piece of pine in it and stepped on the pedal. it would compress =
the pine about what you'd expect from swinging a ten lb without a lot of =
oomph behind it.
DragonsWatch <[email protected]> wrote:Hi Mike,
What is the total weight of your ram/counter weight? Do you figure you are =
getting a comparable blow to another TH with the same weight?
Inquiring minds want to know :-)
Thanks,
Larry
Mike Sweany wrote:
> I did see a sesaw/counterweight style treadle hammer last weekend .
>
> Upright, hammer arm was mounted at and angle to the upright, bush down =
on treadle, whack. Counterbalance returns the hammer head for the next =
blow.
>
> Not fast not elegant but it will sure deliver a good whack. the anvil =
was adjustable in height to maintain a square blow .
>
>
>
> ---------------------------------
> Do you Yahoo!?
> Yahoo! Mail Plus - Powerful. Affordable. Sign up now
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed. To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge=20
> theforge mail list group photo site is
> http://www.photoaccess.com=20
> Login: [email protected]=20
> password: anvil
> ___________
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge=20
theforge mail list group photo site is
http://www.photoaccess.com=20
Login: [email protected]=20
password: anvil
___________
---------------------------------
Do you Yahoo!?
Yahoo! Mail Plus - Powerful. Affordable. Sign up now
--- StripMime Report -- processed MIME parts ---
multipart/alternative
text/plain (text body -- kept)
text/html
The reason this message is shown is because the post was in HTML
or had an attachment. Attachments are not allowed. To learn how
to post in Plain-Text go to: http://www.expita.com/nomime.html ---
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge=20
theforge mail list group photo site is
http://www.photoaccess.com=20
Login: [email protected]=20
password: anvil
___________