what flux? salt, borax, sand?
Bruce Freeman <[email protected]> wrote:It seems to me that insulating firebrick is diatomaceous earth + enough flux to bind it together when it is fired. Anyone know more about this? I was wondering if we might have a short-cut (or cheap-cut) here.
Bruce
NJ
>>> [email protected] 02/05/03 07:09PM >>>
If you want insulating firebrick, the construction grade won't do. You
want the lighter ones that weigh 3 1/2 pounds, or less. Try a ceramic
supply house. They are used for building ceramic kilns.
Ken Zastrow
the copper heron forge
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: [email protected]
password: anvil
___________
---------------------------------
Do you Yahoo!?
Yahoo! Mail Plus - Powerful. Affordable. Sign up now
--- StripMime Report -- processed MIME parts ---
multipart/alternative
text/plain (text body -- kept)
text/html
The reason this message is shown is because the post was in HTML
or had an attachment. Attachments are not allowed. To learn how
to post in Plain-Text go to: http://www.expita.com/nomime.html ---