[TheForge] Phlip--using charcoal in your forge
Roger R Degner
[email protected]
Wed Feb 5 20:43:00 2003
Most buy charcoal before it has been ground up and made into briquettes or
make there own.
One of the guild of metalsmith members from Minnesota made an enormous pile
from soft wood charcoal one batch at a time I believe in a 30 gal barrel. I
have a copy of the directions somewhere but not sure where at the moment
Roger R Degner
Franklin,Minn,USA
----- Original Message -----
From: Lou Polsinelli <[email protected]>
To: <[email protected]>
Sent: Wednesday, February 05, 2003 4:41 PM
Subject: [TheForge] Phlip--using charcoal in your forge
>
> Phlip:
> I would be interested in hearing about using charcoal
> in your forge. Please tell me what kind of charcoal
> you buy, how fast you go through it, adjustments to
> the way you tend the fire, etc.