I used an automotive valve spring the first time (1972 small block chevy) and it started to lose it's "spring". I found some die springs in the McMaster Carr catalog and they work great. They are a little more heavy duty, and you can get them with various inside diameters, and heights.
Phil Rosche
Summerville, SC
>Get a 'valve spring' from your local big truck repair place.
>dave m
>
>
>> A spring is what I had in mind, per my first email. I haven't figured
>> out a good way to use an air cushion. Ideas welcome.
>>
>> So the problem is that it takes quite a spring. Springs are expensive.
>> Anyone know of an inexpensive source?
>>
>> Steve Smith
>>
>
>