The Kinyon plans are sold on the ABANA web site
(www.abana.org). Two other good sites with info are:
http://afc.abana-chapter.com/air_hammer.html
http://www.geocities.com/zoellerforge/hammer.html
Phil Rosche
Summerville, SC
--- Daniel Kretchmar <[email protected]> wrote:
> Can someone tell where I can buy plans for an air
> hammer?
>
> Daniel Kretchmar
> www.irontreeworks.com
>
> Isn't sanity really just a one trick pony, anyway? I
> mean, all you get is one
> trick, rational thinking! But when you're good and
> crazy�ooh hoo hoo hoo�the
> sky's the limit!
> The Tick
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
__________________________________
Do you Yahoo!?
Protect your identity with Yahoo! Mail AddressGuard
http://antispam.yahoo.com/whatsnewfree