Howdy folks, I know this has cropped up before but what are the recipes
for lining a cast iron portable forge. I know some think it is
unneccessary but I'll be lighting this puppy up in cold shop usually and
I don't want to crack the pan. Also I don't think I need to line the
firepot either. The forge is an old buffalo forge cast iron deal with
the side arm to hold the blower. Any advice appreciated.
Cheers
Ron Bakerian