Xylene vapor is not good for your liver ...
-----Original Message-----
From: Shannell Sugrue [mailto:[email protected]]
Sent: Wednesday, December 10, 2003 8:46 AM
To: [email protected]
Subject: Re: [TheForge] incralac - Bronze finishes
I use it on steel, its pretty good, seems to dry quite thin though, =
hardly
looks like there is anything on the bare metal, need a few coats too for
good protection, dries fast, smells nasty (xylene based I think, is that =
bad
stuff?)