[TheForge] MG 750 welding rod

Phil Rosche [email protected]
Fri Dec 5 08:03:03 2003


John:

I haven't used the MG 710, but a guy I know up in
Nebraska, Bob Seward (who's no longer with us) used
them quite a bit for anivl repair.  I've had a few
anvils we re-freshed and they all had hard edges and
the weld material matched the "color" of the face of
the anvil very well.

Phil Rosche 
Summerville, SC
--- John Chobrda <[email protected]> wrote:
>     I learned about using MG 750 for anvil repairs
> from this list, and 
> have had good results with it. Yesterday while I was
> at the dealer, I 
> picked up a copy of Messer's book "Superior alloys
> for maintenance and 
> repair" while reading it I came across MG 710, which
> it states "Ideal 
> for repair and build-up of anvils...". I would like
> to know if anyone on 
> this list has used this rod (it comes as rod, tig
> rod, and mig wire) and 
> if so, what kind of results did you have with it?
> Thanks in advance
> John C.
> 
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
> 
> 


__________________________________
Do you Yahoo!?
Protect your identity with Yahoo! Mail AddressGuard
http://antispam.yahoo.com/whatsnewfree