Good point, Tom. I was focused on the angle rather than where the flame
ended up.
Steve
[email protected] wrote:
>>From: Steve Smith <[email protected]>
>>I used to have a 12"d x 18" forge--two
>>burners was plenty. I used to point them tangent to the internal wall
>>insulation (that swirl effect), but I find pointing them at the floor
>>works just as well. I can't see pointing them up having any benefit.
>
>
> Dear Steve,
>
> The huge benefit from pointing any burners at the ceiling of any furnace is
> to minimize blowing oxygen-rich gases directly at the surface of the
> material being heated, thereby minimizing scale. The flame heats the
> ceiling, then the ceiling heats the work via radiation, and you have much
> less scale.
>
> Tom Troszak
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>