[TheForge] Ed- heat treating S-7

Mike Linn [email protected]
Thu Aug 28 18:52:05 2003


Typically I heat it up to bright cherry into orange and then let it air 
cool. No tempering

I've been using it that way for about 4 years and had no problems. (Hot 
work only)

mike



>One more time ( I know this has been kicked around on the list, but I'll
>save it this time- Promise!)
>What are the basics of heat treating S-7? I have accumulated a bunch of
>round stock...
>Thanks!
>Andy G.


            Mike Linn
      Artist Blacksmith
          McCalla, AL
        AFC Webmaster
http://afc.abana-chapter.com

Some people are like Slinkies...not really good for
anything, but you still can't help but smile when you
see one tumble down the stairs.