old lectricians trick. coil em in figure 8's
On a cart or truck make a bracket a half section of 4" or 6" pipe top and bottom a ft or so apart with a flat plate stop frant and back of the pipe to keep the coils on . sorta like an overgown roller chain link.
Shannell Sugrue <[email protected]> wrote:
Anyone got any good tricks for tidy ways to keeps welding leads from
tangling? Ive just put my tig/arc/plasma box on top of my mig cart, its a
good idea as I now have an all in one, portable welding station but what a
mess the leads get in, there are 6 leads and the 2 power cables, what Id
like is something like the recoiling airhose/water etc housings you can get,
those are really expensive though, anyone ever made their own? failing that
mabey some sort of swing arm or something?.....
Anyone got any tricks to pass on?
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: [email protected]
password: anvil
___________
---------------------------------
Do you Yahoo!?
Yahoo! SiteBuilder - Free, easy-to-use web site design software
--- StripMime Report -- processed MIME parts ---
multipart/alternative
text/plain (text body -- kept)
text/html
The reason this message is shown is because the post was in HTML
or had an attachment. Attachments are not allowed. To learn how
to post in Plain-Text go to: http://www.expita.com/nomime.html ---