>When quenching for hardness, the critical thing is the length of time it
>takes to cool the piece, not the quench medium. A very thin piece of W1
>could be air quenched with good results.
>Darrell
Then it would stand to reason that if you weren't getting the desired
results for which the W-1 is known for when quenching in oil, then why
quench in oil instead of water?
Dave Brown