[TheForge] RE: Frying pan
Andrew Vida
[email protected]
Wed Aug 20 15:16:05 2003
On Wed, 20 Aug 2003 12:21:08 -0500, Bob Ehrenberger <[email protected]>
wrote:
> Phil,
>
> here is the add as in the BAM news letter:
>
> Heavy duty frying pan blanks: Steel, aprox 9"in diam with 2" sides. 12
> ga.
> or 14 ga. with or without 2 3/16 holes for handle. 1-4 $9, 5-9 $8 10+ $7.
> shipping $4 = $.50 ea pan. Contact:
>
OK, I will start by saying I'm not a gourmet cook, so I may be
talking through the wrong sphincter. 12 ga. seems a bit light. All
the really good frying pans I've seen were perhaps 10 to 8 ga, or if
the sides are to be thin as 14 ga., the bottoms are often very heavy
in the 3/16 to 1/4 inch range. Then you have those with copper clad
bottoms and all that, but that may be more work than you're wanting
to get into.