A> ...isn't so much the water content as the Caking inhibitor ingredient...

B> I sent a note to Dial Corp...The reply stated emphatically that not
B> only does it NOT have any "caking inhibitor", it never has.

So today was grocery shopping day.  I bought a brandy new box of 20
Mule Team borax.  It's lumpy.  So much for caking inhibitor. :-)

- Mike

-- 