> Ralph - you are absolutely correct. There are no anti-caking additives or
> any other kind of additive. Boraxo, on the other hand, is a different
> matter, not to mention the Borateem product that doesn't contain any
borax.
>
> According to Dial Corp (producers of the line) - and I quote: "100%
> Borax, a naturally occurring mineral composed of sodium, boron, oxygen and
> water. That's it! "
>
> What is it, you ask? Na2B4O7 -10H2O, Hydrated sodium borate. Heat it up
> and you can drive off the H2O leaving anhydrous borax behind. That's what
> happens when you put 20 Mule Teem on your hot steel, it fluffs up as the
> water is driven off, then promptly melts to do it's fluxing.
>
> Dave Brown
> Heritage Smithing
> Green Bay, WI