How can you say 20 Mule Team is "inferior as a flux.." with so many
sucessful
years (decades) of forge welding?



dan tull
georgia
abba, afc, S.C. psba, obg,sofa
----- Original Message ----- 
From: "Grover Richardson" <[email protected]>
To: <[email protected]>
Sent: Thursday, August 14, 2003 12:55 PM
Subject: RE: [TheForge] Re: Rust,pickling


> Why?
>
> >
>
> > Try to get pure borax, not the 20 mule team type of household borax.
> > The caking inhibitors in it tend to make it inferior as a fluxing
> compound.
> > Chuck