In the situation of having riveted legs, I have not welded the ring but put
the joint for the ring between the two rivets at the top of a leg. The leg,
essentially, holds the ring together. The ring size is a bit more accurate
that way as well.
Ray Baker
Frontier Forge
----- Original Message -----
From: "Bob Rackers" <[email protected]>
To: <[email protected]>
Sent: Wednesday, August 06, 2003 3:54 AM
Subject: RE: [TheForge] 36" diameter ring
> Dan -
>
> I plan to use rivets as well.
> It will have three legs, and I planned to run rivets through one leg and
the
> weld just for extra insurance. The other two legs will be riveted as well.
>
> Bob
>
> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]]On Behalf Of Dan Scheid
> Sent: Wednesday, August 06, 2003 1:10 AM
> To: [email protected]
> Subject: Re: [TheForge] 36" diameter ring
>
>
> Rivet
> Dan Scheid
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>
>