[TheForge] 36" diameter ring
Bob Rackers
[email protected]
Tue Aug 5 22:41:59 2003
Dan -
What option are you proposing other than forge-welding?
Bob
-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Dan Tull
Sent: Tuesday, August 05, 2003 10:33 PM
To: [email protected]
Subject: Re: [TheForge] 36" diameter ring
dan tull
georgia
abba, afc, S.C. psba, obg,sofa
----- Original Message -----
>
> So Kevin, how do you determine how much is the right amount to pull each
time?
> Do you check it after the first pull or two, then adjust from there?
>
Draw a fullsize circle on the layout table or floor, and check often.
To hold a kettle, why forge weld?