[TheForge] Anvil Refacing

[email protected] [email protected]
Sun Aug 3 10:19:01 2003


>> > MG750 rod. from MG Industries, for the rock crushing industry,
>> "highest impact"resistance
>Sure wish somebody in this part of the country (northwest coast) knew what
>it was...What do we do- mail order it?
>None of the welding shops carry it.
>Andy G.



Andy,

A quick search sent me here.

http://216.239.37.104/search?q=cache:FI0K9Qz8KewJ:www.amfiller.com/npdf/maintenancealloys.pdf+MG+750+weld+rod&hl=en&ie=UTF-8

It's a cross reference guide that shows some other mfgs of the MG750.