>Thanks Dan, but yours isn't what we are using at the event. Flaxy is coming
>up to teach us about Medieval Period iron making & we are building a clay
>Scandinavian Shaft furnace type of bloomery, very low tech & no metal on
>the outside. When I have some time I would love to discuss yields & such,
>but I am looking for some photos to show the Fire Chief tomorrow. The
>photos that were shown had on the Forge had Flaxy in them (I would get some
>from her but she doesn't check her email very often).